• Grade 201 stainless steel has good formability, corrosion resistance, and fabricability. 201 is a low cost alternative to the conventional Cr-Ni austenitic stainless steels, such as stainless 304. Copper is added to compensate for the increased work-hardening rate. Stainless steel 201 has relatively lower ductility and formability compared to stainless steel 304.
Steel grades | 201 |
Production | cold rolled |
Thickness | 0.2-3.0mm |
EDiameter | 80-700mm |
Finishes | 2B,BA |
Film | Paper,PE |
packing | Water-proof wooden package |
Application | Kitchenware,Utensil |
Payment terms | T/T and L/C at sight |
Delivery time | 20-30 days, it depends on the quantity. |
Chemical composition
Grade | %C | %Si | %Mn | %P | %S | %Cr | %Ni | %Cu |
201 J4 | 0.069 | 0.37 | 9.48 | 0.038 | 0.001 | 14.62 | 1.16 | 1.56 |
201 J1 | 0.105 | 0.44 | 10.12 | 0.037 | 0.005 | 13.88 | 1.2 | 0.83 |
201 J3 | 0.138 | 0.35 | 9.19 | 0.036 | 0.001 | 14.56 | 1.09 | 0.59 |
201 J2 | 0.138 | 0.041 | 8.44 | 0.04 | 0.002 | 14.42 | 1.15 | 0.35 |
201 J5 | 0.146 | 0.441 | 9.052 | 0.054 | 0.005 | 13.21 | 1.407 | 0.239 |